Titanium Metal Sheeting: Hard Stainless

From ATITD7
Revision as of 12:34, 27 January 2016 by Flowbar (talk | contribs)
Jump to navigationJump to search

This is a very easy treatment. Here is a basic recipe:

  • 100 Titanium
  • 2 Lime to increase strength and lower corrosion
  • 1 Coal to increase strength further, will also unfortunately increase corrosion back
  • 2 Cactus Sap to peak strength to Hard, will also lower corrosion
  • 1 Gravel to lower corrosion, will lower strength a little
  • 2 Potash to push corrosion down to Stainless, will hardly affect strength

First add 100 Titanium to the bath. Then run 10s each for the ingredients above, like this:

  • Lime 20s
  • Coal 10s
  • Cactus Sap 20s
  • Gravel 10s
  • Potash 20s

Different Chemical Baths behave slightly different, but the basic idea above still applies. Here is how to modify the recipe:

  • If, after applying the Cactus Sap, strength is not almost fully "Hard", it might drop too low when applying Gravel later. Increase Cactus Sap to 30s in that case.
  • If 20s of Potash treatment is not enough to get "Stainless", add another 10s of Potash.
  • It is possible to replace 1 unit/10 seconds of Potash with 1 unit/10 seconds of Arsenic directly after the Gravel.
  • It is possible to skip Lime and instead increase the time using Coal or Cactus Sap to get the
  • It might be possible to run first a lot of Cactus Sap, or Coal and then Cactus Sap, to peak strength and then a lot of Potash to push down corrosion, but Potash is expensive, and this has not been tested yet.

Sheetings take 2 units of treated metal and take 2 minutes to cool in a Forge upgraded with a pair of Pinch Rollers